3:33
If it's as good, then why haven't we been using it for all these years?
3:38
So we've been using low silver maybe 15 years ago or so when we had eutectictin sac alloy or eutectictin silver.
3:50
And then everybody for waves specifically were looking for low silver.
3:55
And then...
3:57
The attention shifted to higher reliability.
4:01
Alloy and silver helps a lot with wetting and thermocycling reliability.
4:06
And low silver was forgotten.